Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Wanhua Chemical Wanthane® WHT-1495B Polyester Based TPU

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane TPE , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer Wanhua Chemical Group Co., Ltd.
Trade Name Wanthane®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wanhua Chemical Wanthane® WHT-1495B Polyester Based TPU.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Good extrusion stability, high transparency, excellent mechanical propertiesInformation provided by Wanhua Chemical Group Co., Ltd.
Physical Properties Metric English Comments
Density 1.21 g/cc
0.0437 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 97
97
ASTM D2240
Hardness, Shore D 62
62
ASTM D2240
Tensile Strength 35.0 MPa
5080 psi
ASTM D412
Elongation at Break 440 %
440 %
ASTM D412
100% Modulus 0.0150 GPa
2.18 ksi
ASTM D412
300% Modulus 0.0280 GPa
4.06 ksi
ASTM D412
Tear Strength 170 kN/m
970 pli
ASTM D624
Abrasion 170
170
Abrasion resistance, mm<sup>3</sup>; ISO 4649
Processing Properties Metric English Comments
Processing Temperature 190 - 210 °C
374 - 410 °F
Users viewing this material also viewed the following: