Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Wanhua Chemical Wanthane® WHT-1172 Polyester Based TPU

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane TPE , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer Wanhua Chemical Group Co., Ltd.
Trade Name Wanthane®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wanhua Chemical Wanthane® WHT-1172 Polyester Based TPU.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Excellent mechanical properties, high abrasion resistance, tear resistance, short cycle timeInformation provided by Wanhua Chemical Group Co., Ltd.
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength 43.0 MPa
6240 psi
ASTM D412
Elongation at Break 350 %
350 %
ASTM D412
100% Modulus 0.0280 GPa
4.06 ksi
ASTM D412
300% Modulus 0.0370 GPa
5.37 ksi
ASTM D412
Tear Strength 220 kN/m
1260 pli
ASTM D624
Abrasion 42
42
Abrasion resistance, mm<sup>3</sup>; ISO 4649
Processing Properties Metric English Comments
Processing Temperature 200 - 220 °C
392 - 428 °F