Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Victrex® Vicote® F816 Black Polyetheretherketone (PEEK) Liquid Dispersion

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK)
Manufacturer Victrex
Trade Name Vicote®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Victrex® Vicote® F816 Black Polyetheretherketone (PEEK) Liquid Dispersion.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
VICOTE® is the brand name for the Victrex range of coatings. VICOTE Coatings are available through Victrex or its preferred coater network. The VICOTE F815 and F816Blk grades have been specifically formulated to provide a coating that gives high wear and abrasion resistance combined with excellent release properties that are retained as the coating wears. These properties are retained at high temperatures where other release coatings would potentially fail. VICOTE dispersions have a low level of extractables..All information provided by Victrex.
Physical Properties Metric English Comments
Storage Temperature 5.00 - 25.0 °C
41.0 - 77.0 °F
Mechanical Properties Metric English Comments
Impact 1.0
1.0
1m, 2kg, Indent 5mm; ISO 6272
Coefficient of Friction 0.15
0.15
µm @ 10 min., Using 250N Load; ASTM G 133
Processing Properties Metric English Comments
Drying Temperature 120 °C
248 °F
overnight before use
150 °C

@Time 10800 sec
302 °F

@Time 3.00 hour
Descriptive Properties Value Comments
Color Black
Konig Hardness (seconds) 116
ISO 1522
Users viewing this material also viewed the following: