Vicone High Performance Rubber VicoFluro™ 106F-BK High Performance Fluoroelastomer

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer Vicone High Performance Rubber
Trade Name VicoFluro™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Vicone High Performance Rubber VicoFluro™ 106F-BK High Performance Fluoroelastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Vicone
Physical Properties Metric English Comments
Density 1.852 g/cc
0.06691 lb/in³
ASTM D3165
Mechanical Properties Metric English Comments
Hardness, Shore D 61
61
ASTM D2240
59.41

@Treatment Temp. 200 °C,
Time 252000 sec
59.41

@Treatment Temp. 392 °F,
Time 70.0 hour
Heat Aging; ASTM D573
Tensile Strength, Yield 10.8 MPa
1570 psi
ASTM D412
11.99 MPa

@Treatment Temp. 200 °C,
Time 252000 sec
1739 psi

@Treatment Temp. 392 °F,
Time 70.0 hour
Heat Aging; ASTM D573
Elongation at Break 273.2 %
273.2 %
ASTM D412
191.24 %

@Treatment Temp. 200 °C,
Time 252000 sec
191.24 %

@Treatment Temp. 392 °F,
Time 70.0 hour
Heat Aging; ASTM D573
Compressive Modulus 0.000300 GPa

@Strain 5.00 %
0.0435 ksi

@Strain 5.00 %
0.000610 GPa

@Strain 10.0 %
0.0885 ksi

@Strain 10.0 %
0.00122 GPa

@Strain 20.0 %
0.177 ksi

@Strain 20.0 %
0.00171 GPa

@Strain 25.0 %
0.248 ksi

@Strain 25.0 %
Compression Set 6.5 %

@Temperature 175 °C,
Time 79200 sec
6.5 %

@Temperature 347 °F,
Time 22.0 hour
ASTM D395
Descriptive Properties Value Comments
Color Black