Universal Wire Works ER90SB-9 Stainless Steel Bare Wire

Category Metal , Ferrous Metal , Stainless Steel
Manufacturer Universal Wire Works
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Universal Wire Works ER90SB-9 Stainless Steel Bare Wire.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This alloy is a 9 percent chromium, 1 percent molybdenum solid wire modified with niobium (columbium) and vanadium designed to provide strength, toughness, fatigue life, oxidation resistance and corrosion resistance at elevated temperatures. Due to the higher elevated temperature properties of this alloy, compositions that are now fabricated from stainless steels and ferritic steels may be fabricated from a single alloy, eliminating problems associated with dissimilar welds.Information provided by Universal Wire Works for their line of welding wire and filler metal.
Component Elements Properties Metric English Comments
Chromium, Cr 9.0 %
9.0 %
Iron, Fe 90 %
90 %
As Remainder
Molybdenum, Mo 1.0 %