Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Universal Wire Works BCo-1 (AMS 4783) Nickel Base Brazing Filler Metal

Category Metal , Nonferrous Metal , Cobalt Alloy , Solder/Braze Alloy
Manufacturer Universal Wire Works
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Universal Wire Works BCo-1 (AMS 4783) Nickel Base Brazing Filler Metal.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Universal Wire Works for their line of welding wire and filler metal.
Thermal Properties Metric English Comments
Melting Point 1107 - 1150 °C
2025 - 2100 °F
Solidus 1107 °C
2025 °F
Liquidus 1150 °C
2100 °F
Component Elements Properties Metric English Comments
Boron, B 0.80 %
0.80 %
Chromium, Cr 19 %
19 %
Cobalt, Co 50 %
50 %
Nickel, Ni 17 %
17 %
Silicon, Si 8.0 %
8.0 %
Tungsten, W 4.0 %
4.0 %