Category Ceramic
Manufacturer Unifrax I LLC
Trade Name Fiberfrax®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Unifrax Fiberfrax® Pumpable-GS Pumpable Insulation.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Fiberfrax Pumpable-LDS, Pumpable-GS, and Topcoat 2600 Insulating Mix were designed for application into difficult-to-reach areas requiring insulation. Fiberfrax Pumpable-LDS and Pumpable-GS have temperature grade ratings of 1260°C (2300°F). Fiberfrax Topcoat 2600 Insulating Mix has a temperature grade rating of 1426°C (2600°F). A conventional air-operated extrusion pump permits application of these products directly from their container into furnace and boiler hot spots, refractory cracks, furnace door jambs, and other areas requiring high-temperature insulating and sealing.Typical ApplicationsOn-line boiler hot spot repairsSeal surface door jambsSeal furnace penetrationsSeal around burner blocksCaulk refractory cracksOn-line refractory hot spot repairsTurbine exhaust duct hot spot repairsInformation Provided by Unifrax I LLC
Physical Properties Metric English Comments
Density 0.400 g/cc
0.0145 lb/in³
Dry
1.12 g/cc
0.0405 lb/in³
Wet
Solids Content 28 %
28 %
Loss On Ignition 3.0 - 4.0 %
3.0 - 4.0 %
Mechanical Properties Metric English Comments
Modulus of Rupture 0.00241 GPa
0.350 ksi
Dry
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1093 °C
1999 °F
Recommended Operating Temperature
Shrinkage 6.0 %

@Temperature 1090 °C,
Time 86400 sec
6.0 %

@Temperature 1990 °F,
Time 24.0 hour
Descriptive Properties Value Comments
Appearance Smooth putty
Molten Aluminum Wetting Resistance Good
Temperature Grade (°F) 2300