Trelleborg Emerson & Cuming Eccobond® 26 Two-Component General Purpose Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Trelleborg Emerson & Cuming, Inc.
Trade Name Eccobond®
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Trelleborg Emerson & Cuming Eccobond® 26 Two-Component General Purpose Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Emerson & Cuming 26 Eccobond® Two-Component General Purpose Epoxy AdhesiveFilled, room temperature curing, general purpose, epoxy adhesive. Recommended for varied uses including repair and manufacture of tools, furniture, boats, and electronic sub-assemblies. Mix Ratio of 100:100. Bonding Type: Epoxy
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
Mechanical Properties Metric English Comments
Adhesive Bond Strength 14.5 MPa
2100 psi
Processing Properties Metric English Comments
Cure Time 19.8 min

@Temperature 65.0 °C
0.330 hour

@Temperature 149 °F
240 min

@Temperature 25.0 °C
4.00 hour

@Temperature 77.0 °F
Descriptive Properties Value Comments
Color Off-white
Viscosity Thixotropic Paste