Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Henkel Hysol EA 9686 Film Adhesive

Category Polymer , Adhesive , Film , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Henkel
Trade Name Hysol
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Henkel Hysol EA 9686 Film Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Second generation, moisture resistant, toughened 250°F / 121°C curing film with service performance to 300°F / 149°C. Excellent for composite or metal bonding. Data from .060 psf, 300 g / m2.Applications: Composite Bonding Metal and Honeycomb Bonding Composite Surfacing
Physical Properties Metric English Comments
Storage Temperature -18.0 °C
-0.400 °F
Mechanical Properties Metric English Comments
Tensile Strength 6.90 MPa
1000 psi
Flatwise
Adhesive Bond Strength 6.90 MPa

@Temperature 149 °C
1000 psi

@Temperature 300 °F
Lap Shear
40.0 MPa

@Temperature -55.0 °C
5800 psi

@Temperature -67.0 °F
Lap Shear
40.0 MPa

@Temperature 25.0 °C
5800 psi

@Temperature 77.0 °F
Lap Shear
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 149 °C
300 °F
Glass Transition Temp, Tg 133 °C
271 °F
dry
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 121 °C
1.00 hour

@Temperature 250 °F
Descriptive Properties Value Comments
Honeycomb Climbing Drum Peel, mN/m 76
at 25°C
Out-Time (days) 90
at 25°C