Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Tra-Con Tra-Duct 2919 Room Temperature Conductive, Flexible Silver Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy, Electrically Conductive , Filled/Reinforced Thermoset
Manufacturer Tra-Con, Inc.
Trade Name Tra-Duct
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tra-Con Tra-Duct 2919 Room Temperature Conductive, Flexible Silver Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
TRA-DUCT 2919 is a non-bleeding, electrically conductive, silver-filled epoxy formulation recommended for electronic bonding, coating, and sealing applications that require high flexibility coupled with good electrical and mechanical properties. This two-part, thixotropic adhesive of refined pure silver and epoxy resin components is free of solvents and copper or carbon additives. It develops resilient, electrically and thermally conducting bonds and coatings between many different and dissimilar materials such as metals, ceramics, glass and plastic insulates. TRA-DUCT 2919 cures at room temperature and can be used as a flexible "cold-solder" for heat-sensitive components where hot-soldering is impractical. It also can be used for the assembly and repair of electrical modules, flexible circuits, membrane switches, wave guides, flat cable and high frequency shields. Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Specific Gravity 2.32 g/cc
2.32 g/cc
Mixed
Solids Content 100 %
100 %
Reactive Solids Content
Volatile Organic Compounds (VOC) Content 24.41 g/l
24.41 g/l
Viscosity 995000 cP

@Temperature 25.0 °C
995000 cP

@Temperature 77.0 °F
Mixed (sp #T-F, 10 rpm)
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
4 hrs @ 65°C
Adhesive Bond Strength 0.621 MPa
90.0 psi
Lap shear, alum to alum, 24 hrs @ 25°C
1.17 MPa
170 psi
Lap shear, alum to alum, 4 hrs @ 65°C
Thermal Properties Metric English Comments
CTE, linear 35.0 µm/m-°C

@Temperature 20.0 °C
19.4 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 1.60 W/m-K
11.1 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 110 °C
230 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Glass Transition Temp, Tg 4.00 °C
39.2 °F
Ultimate Tg
Electrical Properties Metric English Comments
Volume Resistivity 0.00011 ohm-cm
0.00011 ohm-cm
cured 4 hrs @ 65°C
0.0016 ohm-cm
0.0016 ohm-cm
cured 24 hrs @ 25°C
Processing Properties Metric English Comments
Cure Time 240 min

@Temperature 65.0 °C
4.00 hour

@Temperature 149 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Pot Life 30 min
30 min
Descriptive Properties Value Comments
Color Silver
Mix Ratio, parts by weight 90/100
Resin/Hardener
Thixotropic Index 4.9
5 rpm/50 rpm
Users viewing this material also viewed the following: