Material Notes:
TRA-BOND 293-1.5T general purpose epoxy adhesive is designed to provide strong, semi-rigid bonds to a variety of difficult-to-bond substrates, such as gold, nickel, silver, copper, and brass. This version of the 293-series is more flexible. The 293-series of adhesives cures at moderate temperatures, 60°C to 75°C. Information provided by Tra-Con Inc.
Mechanical Properties Metric English Comments
Adhesive Bond Strength 26.2 MPa
3800 psi
Lap shear, silver to silver
27.6 MPa
4000 psi
Lap shear, gold to gold
27.6 MPa
4000 psi
Lap shear, brass to brass
37.9 MPa
5500 psi
Lap shear, alum to alum
Processing Properties Metric English Comments
Cure Time 45.0 min

@Temperature 120 °C
0.750 hour

@Temperature 248 °F
90.0 min

@Temperature 95.0 °C
1.50 hour

@Temperature 203 °F
240 min

@Temperature 75.0 °C
4.00 hour

@Temperature 167 °F
1440 min

@Temperature 60.0 °C
24.0 hour

@Temperature 140 °F
Shelf Life 12.0 Month

@Temperature -40.0 °C
12.0 Month

@Temperature -40.0 °F
Descriptive Properties Value Comments
Color Black
Working Life hours 8