| Category | Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP |
| Manufacturer | Toyobo |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Toyobo A1061D Thermoplastic Polyurethane Elastomer, Injection Grade.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.22 g/cc | 0.0441 lb/in³ | ASTM D792 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 61 | 61 | ASTM D2240 |
| Tensile Strength, Ultimate | 46.0 MPa | 6670 psi | ASTM D638 |
| Tensile Strength, Yield | 20.6 MPa <br>@Strain 100 % |
2990 psi <br>@Strain 100 % |
ASTM D638 |
| Elongation at Break | 450 % | 450 % | ASTM D638 |
| Tear Strength | 216 kN/m | 1230 pli | ASTM D624 |
| Taber Abrasion, mg/1000 Cycles | 70 | 70 | H22 |
| Compression Set | 40 % | 40 % | ASTM D395B |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Vicat Softening Point | 135 °C | 275 °F | ASTM D1525 |
| Brittleness Temperature | <= -65.0 °C | <= -85.0 °F | ASTM D746 |