Total Finathene® WR 201 B HDPE blow molding  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total Finathene® WR 201 B HDPE blow molding  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FINATHENE® WR 201 B is a high density polyethylene produced by the slurry loop low pressure polymerization process. FINATHENE® WR 201 B has been developed for the blow molding of Plastic Fuel Tanks and automotive technical parts. FINATHENE® WR 201 B is suitable for the most common barrier treatments. The material specific characteristics allow to achieve outstanding tank properties, including crash test and fire resistance, with a substantial net weight reduction of the Plastic Fuel Tank.Information provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Density 0.9495 g/cc
0.03430 lb/in³
ISO 1183
Thermal Stress Crack Resistance >= 250 hour
>= 250 hour
ASTM D 1693
Melt Flow 8.0 g/10 min

@Temperature 190 °C
8.0 g/10 min

@Temperature 374 °F
High Load; ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 25.0 MPa
3630 psi
ISO 527
Elongation at Yield 11 %
11 %
ISO 527
Flexural Modulus 1.10 GPa
160 ksi
ISO 178