Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow Corning Z-1221 PHENYLMETHYLDICHLOROSILANE

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Dow Corning
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning Z-1221 PHENYLMETHYLDICHLOROSILANE.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
Kinematic Viscosity 1.6 cSt
1.6 cSt
Molecular Weight 191.1 g/mol
191.1 g/mol
Thermal Properties Metric English Comments
Boiling Point 35.0 °C
95.0 °F
Flash Point 72.2 °C
162 °F
closed cup
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance colorless
Users viewing this material also viewed the following: