| Category | Polymer |
| Manufacturer | Teknor Apex Company |
| Trade Name | TruVis Esters™ |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Teknor Apex TruVis Esters™ TNTM TriNonyl Trimellitate.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 0.983 g/cc | 0.983 g/cc | |
| Viscosity | 10.2 cP @Temperature 100 °C |
10.2 cP @Temperature 212 °F |
|
| 91.9 cP @Temperature 40.0 °C |
91.9 cP @Temperature 104 °F |
||
| Viscosity Measurement | 90.0 | 90.0 | Viscosity Index |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Pour Point | -35.0 °C | -31.0 °F | |
| Flash Point | 274 °C | 525 °F |
| Chemical Properties | Metric | English | Comments |
|---|---|---|---|
| Acid Value | <= 0.10 | <= 0.10 | mg KOH/g |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Appearance | Clear | |
| Color | 100 | Pt/Co Scale |
| Ester Content (%), min | 99 | |
| Moisture (ppm), max | 500 |