Thermoseal RG-S160 PTG Gasketing

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Styrene Butadiene Rubber
Manufacturer Thermoseal Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Thermoseal RG-S160 PTG Gasketing.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Thermoseal RG-S160 offers exceptional sealability and crush resistance in a wide range of applications. RG-S160 is composed of a blend of aramid, mineral, and cellulose fibers and graphite and other inorganic fillers with a styrene butadiene binder. A factory applied release coating on both sides aids in flange removal. Continuous roll lengths allow efficient and economical fabrication with high speed die cutting equipment. Typical applications range from power sport and other small engine gaskets to heavy duty diesel service with intermittent operating temperatures up to 550° F (288° C).Information provided by Thermoseal Inc.
Physical Properties Metric English Comments
Density 1.60 g/cc
0.0578 lb/in³
ASTM F1315
Thickness 800 microns
31.5 mil
Thickness tested
Mechanical Properties Metric English Comments
Tensile Strength >= 8.00 MPa
>= 1160 psi
ASTM F152
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 288 °C
550 °F
intermittent
Descriptive Properties Value Comments
Binder Type Styrene Butadiene Rubber
Compressibility 8-20 percent
ASTM F36J
Recovery >40 percent
ASTM F36J
Thickness Increase <60%
After immersion in Oil IRM903
Weight Increase <45%
After immersion in Oil IRM903