Material Notes:
Thermoseal ML-N562 is a synthetic fiber and nitrile butadiene gasket material designed for difficult sealing applications with very low flange pressures or very rough surface finishes. It combines Multi-Layer Technology structure for exceptional low flange pressure sealability and exceptional torque retention together w ith a more compressible core. Multi-Layer Technology sheet products consist of a reinforced high density core w ith conformable sealing layers on each side. ML-N562 provides heat and chemical resistance in coolant, lubricant, and hot air applications. Typical applications include automotive, marine, and small engine applications with intermittent operating temperatures up to 500° F (260° C).Information provided by Thermoseal Inc.
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
ASTM F1315
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 260 °C
500 °F
intermittent
Descriptive Properties Value Comments
ASTM F104 Line Call Out F715121B3E12K6M4
Compressibility >20%
ASTM F36J
Creep <20%
ASTM F38B (1/32")
Pressure <1400 psi
Recovery >50%
ASTM F36J
Sealability <0.20 ml/hr
ASTM F37
Thickness Increase <10%
After immersion in ASTM Oil #1 for 5 hrs at 300°F
<15%
After immersion in Fuel B for 5 hrs at 73°F
Weight Increase <10%
After immersion in Fuel B for 5 hrs at 73°F