Thermoseal KLINGER® top-chem-2005 PTFE Gasketing

Category Polymer , Thermoplastic , Fluoropolymer , PTFE
Manufacturer Thermoseal Inc.
Trade Name KLINGER®
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Thermoseal KLINGER® top-chem-2005 PTFE Gasketing.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Economical alternative w hen service conditions are moderate Suitable for a wide range of applications in the chemical industriesExcellent chemical resistance in strongly acidic applicationsFDA compatibleHolds shape for thermal cyclesPermits/Certifications: KTW proposal; DIN-DVGW permit; FDA conformity; TA-Luft certification and Germanischer LloydInformation provided by Thermoseal Inc.
Physical Properties Metric English Comments
Density 2.00 g/cc
0.0723 lb/in³
Thickness 1500 microns
59.1 mil
Thickness tested
Descriptive Properties Value Comments
Compressibility 7 percent
ASTM F36
Klinger Cold/Hot Compression 10 percent
75°F/3,625 psi
30 percent
480°F/3,625 psi
Recovery 35 percent
ASTM F36
Sealability 0.02 mg/s m
DIN 28090-2
0.2 ml/min
DIN 3535/6
Stress Relaxation 25 MPa
DIN 52913, 16h 4,350 psi, 300°F
Thickness/Weight Increase 2/2%
H2SO4, 100%: 18h/75°F
2/7%
HNO3, 100%: 18h/75°F