Braskem VA2019A EVA Foam Copolymer

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate
Manufacturer Braskem
Trade Name
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Braskem VA2019A EVA Foam Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
The VA2019A is a copolymer of Ethylene-Vinyl Acetate (EVA) with medium vinyl-acetate content. VA2019A is an easy processing product with high compatibility with other thermoplastic and elastomeric resins and mineral loads. Its elasticity is higher than the LDPE of the same MI. It has excellent environmental stress crack resistance (ESCR) and low temperature brittleness. The compounds produced with VA2019A will have lightness, good resistance to deformation, and high retention of color. Crosslinked and/or expanded parts have several applications including: compounds for the footwear (sole, insoles, etc), toys, and gifts industry (produced by injection molding); and polymeric blends.
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
ASTM-D1505 / ASTM-D792
ESCR 100% Igepal® >= 300 hour

@Thickness 2.00 mm,
Temperature 50.0 °C
>= 300 hour

@Thickness 0.0787 in,
Temperature 122 °F
0.3 mm notched-plaques; ASTM-D1693
Vinyl Acetate Content 18 %
18 %
Melt Flow 2.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM-D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 90
90
ASTM-D2240
Hardness, Shore D 31
31
ASTM-D2240
Thermal Properties Metric English Comments
Melting Point 87.0 °C
189 °F
ASTM-D3418
Vicat Softening Point 62.0 °C

@Load 1.02 kg
144 °F

@Load 2.25 lb
ASTM-D1525