Material Notes:
Notes: Terraloy™ BP-10001A is a Thermoplastic Starch/LLDPE ready-to-process compound that contains up to 30% of TPS renewable content. This compound is for blown film application. Forms: Pellets Additional Information: Biobased Content: < 30.0Information Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.01 g/cc
1.01 g/cc
ASTM D792
Water Vapor Transmission 9.00 g/m²/day
0.580 g/100 in²/day
Oxygen Transmission Rate 7140 cc/m²/day
460 cc/100 in²/day
ASTM D1922
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 480 %
480 %
ASTM D882
Film Elongation at Break, TD 680 %
680 %
ASTM D882
Secant Modulus 0.193 GPa
28.0 ksi
MD; ASTM D882
0.288 GPa
41.8 ksi
TD; ASTM D882
Elmendorf Tear Strength MD 320 g
320 g
ASTM D1922
Elmendorf Tear Strength TD 620 g
620 g
ASTM D1922
Dart Drop Test 450 g
0.992 lb
ASTM D1709
Film Tensile Strength at Break, MD 53.0 MPa
7690 psi
ASTM D882
Film Tensile Strength at Break, TD 30.9 MPa
4480 psi
ASTM D882