Teknor Apex APEX® 84468 Polyvinyl Chloride, Flexible

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Flexible Grade , PVC, Wire and Cable Grade
Manufacturer Teknor Apex Company
Trade Name APEX®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex APEX® 84468 Polyvinyl Chloride, Flexible.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Notes: 105°C Jacket; RoHS Compliant Features: Flame Retardant; Good UV Resistance Uses: Cable Jacketing; Insulation Forms: Pellets Agency Ratings: UL 1063; UL 1581; UL 62Information Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.35 g/cc
1.35 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 85
85
15 seconds; ASTM D2240
Tensile Strength at Break 19.7 MPa
2850 psi
ASTM D638
Elongation at Break 360 %
360 %
ASTM D638
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 105 °C
221 °F
Continuous Use; ASTM D794
Brittleness Temperature -28.0 °C
-18.4 °F
ASTM D746
Oxygen Index 31 %
31 %
ASTM D2863
Descriptive Properties Value Comments
Appearance Opaque