Material Notes:
Notes: 105°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain Reliefs; Wire and Cable ApplicationsForms: Pellets Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molded ComponentsAdditional Information: Temperature Rating: 105°CRecognized Component, CSA C22.2 No. 0.6, CSA Flammability Classification: 0.6V-2 at .81 mmInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.39 g/cc
1.39 g/cc
ASTM D792
Linear Mold Shrinkage 0.010 - 0.012 cm/cm
0.010 - 0.012 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore C 82
82
10 seconds; ASTM D2240
Tensile Strength at Break 18.8 MPa
2730 psi
ASTM D638
Elongation at Break 280 %
280 %
ASTM D638
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 105 °C
221 °F
Continuous Use; ASTM D794
Brittleness Temperature -10.0 °C
14.0 °F
ASTM D746
Flammability, UL94 V-0

@Thickness 3.00 mm
V-0

@Thickness 0.118 in
Oxygen Index 31 %
31 %
ASTM D2863
Electrical Properties Metric English Comments
Comparative Tracking Index >= 600 V

@Thickness 3.00 mm
>= 600 V

@Thickness 0.118 in
UL 746
Hot Wire Ignition, HWI >= 120 sec

@Thickness 3.00 mm
>= 120 sec

@Thickness 0.118 in
UL 746
High Amp Arc Ignition, HAI 60 - 120 arcs

@Thickness 3.00 mm
60 - 120 arcs

@Thickness 0.118 in
UL 746
Processing Properties Metric English Comments
Melt Temperature 193 °C
380 °F
Processing Temperature
Descriptive Properties Value Comments
Appearance Opaque