| Category | Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled |
| Manufacturer | Techmer ES |
| Trade Name | Statiblend® |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Techmer ES Statiblend® ABS LE.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.10 g/cc | 0.0397 lb/in³ | ASTM D792 |
| Water Absorption | 0.28 % @Time 86400 sec |
0.28 % @Time 24.0 hour |
ASTM D570 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 112 | 112 | ASTM D785 |
| Tensile Strength, Yield | 50.3 MPa | 7300 psi | ASTM D638 |
| Elongation at Yield | 4.0 % | 4.0 % | ASTM D638 |
| Flexural Yield Strength | 8.96 MPa | 1300 psi | ASTM D790 |
| Flexural Modulus | 3.10 GPa | 450 ksi | ASTM D790 |
| Izod Impact, Notched | 0.534 J/cm @Thickness 3.17 mm |
1.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 84.6 µm/m-°C | 47.0 µin/in-°F | ASTM D696 |
| Deflection Temperature at 1.8 MPa (264 psi) | 96.1 °C | 205 °F | Unannealed; ASTM D648 |
| Flammability, UL94 | HB | HB |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+10 ohm-cm | 1.00e+10 ohm-cm | ASTM D257 |