Material Notes:
Processed by extrusion or injection molding. Elastollan ® 1100 series products are FDA Sec. 177.2600 compliant. Elastollan 1100 series of products are polyether-based thermoplastic polyurethanes. They exhibit excellent low temperature properties, hydrolysis resistance and fungus resistance. These products can be injection and blow molded and extruded. As with all TPU products this grade must be dried prior to processing.Property values below are typical values based on test samples cured 20 hours at 100°C before testing. Information provided by BASF Corporation.
Physical Properties Metric English Comments
Density 1.11 g/cc
0.0401 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
ASTM D2240
Tensile Strength, Ultimate 32.0 MPa
4640 psi
ASTM D412
Tensile Strength, Yield 5.50 MPa
<br>@Strain 100 %
798 psi
<br>@Strain 100 %
ASTM D-412
10.0 MPa
<br>@Strain 300 %
1450 psi
<br>@Strain 300 %
ASTM D-412
Elongation at Break 600 %
600 %
ASTM D412
Tear Strength 90.0 kN/m
514 pli
ASTM D624
Taber Abrasion, mg/1000 Cycles 25
25
H-18 wheel; ASTM D-1044.
Tensile Set 45 %
45 %
at break; ASTM D-412
Electrical Properties Metric English Comments
Electrical Resistivity >= 1.00e+11 ohm-cm
>= 1.00e+11 ohm-cm
DIN 53482/VDE 0303
Surface Resistance >= 1.00e+11 ohm
>= 1.00e+11 ohm
DIN 53482/VDE 0303
Dielectric Constant 6.5
<br>@Frequency 1e+6 Hz
6.5
<br>@Frequency 1e+6 Hz
DIN 53483/VDE 0303
7.6
<br>@Frequency 1000 Hz
7.6
<br>@Frequency 1000 Hz
DIN 53483/VDE 0303
8.0
<br>@Frequency 50 Hz
8.0
<br>@Frequency 50 Hz
DIN 53483/VDE 0303
Dielectric Strength 39.0 kV/mm
991 kV/in
DIN 53481/VDE 0303
Dissipation Factor 0.026
<br>@Frequency 1000 Hz
0.026
<br>@Frequency 1000 Hz
0.087
<br>@Frequency 1e+6 Hz
0.087
<br>@Frequency 1e+6 Hz
0.121
<br>@Frequency 50 Hz
0.121
<br>@Frequency 50 Hz
Comparative Tracking Index >= 600 V
>= 600 V
DIN/IRC 112