Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 18% Filler by WeightFeatures: Flame RetardantAppearance: BlackInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.50 g/cc
0.0542 lb/in³
ASTM D792
Water Absorption 0.70 %

@Time 86400 sec
0.70 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0040 cm/cm

@Thickness 3.17 mm
0.0040 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 111
111
ASTM D785
Tensile Strength, Yield 121 MPa
17500 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Strength 179 MPa
26000 psi
ASTM D790
Flexural Modulus 6.21 GPa
900 ksi
ASTM D790
Izod Impact, Notched 0.641 J/cm

@Thickness 3.17 mm
1.20 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 79.2 µm/m-°C
44.0 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 238 °C
460 °F
Unannealed; ASTM D648
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+9 ohm-cm
1.00e+9 ohm-cm
ASTM D257
Surface Resistance 1.00e+11 ohm
1.00e+11 ohm
ASTM D257
Dielectric Strength 17.3 kV/mm
440 kV/in
Method A (Short-Time); ASTM D149