Taiwan Sheen Soon Sheenthane® D6612R Thermoplastic Polyurethane Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane TPE , Polyurethane, TP
Manufacturer Taiwan Sheen Soon Co. Ltd.
Trade Name Sheenthane®
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Taiwan Sheen Soon Sheenthane® D6612R Thermoplastic Polyurethane Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD.
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
Mechanical Properties Metric English Comments
Hardness, Shore D 63 - 67
63 - 67
Tensile Strength 47.1 MPa
6830 psi
Elongation at Break 350 %
350 %
100% Modulus 0.01762 GPa
2.556 ksi
300% Modulus 0.0373 GPa
5.40 ksi
Processing Properties Metric English Comments
Processing Temperature 210 - 230 °C
410 - 446 °F