TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR N990 Filler

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer TSE Industries, Inc
Trade Name Millathane®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR N990 Filler.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subjected to high wear in service. It has a unique combination of excellent properties, such as low temperature characteristics, and resistance to heat deterioration, ozone cracking, weathering and swelling in oils or solvents.FormulationMillathane CM 100.0N99020.0Coumarone-Indene Resin6.67MBTS4.0MBT1.0Sulfur0.75CAYTUR 40.35Zinc Stearate0.50All information provided by TSE Industries
Physical Properties Metric English Comments
Specific Gravity 1.15 g/cc
1.15 g/cc
Mooney Viscosity 21

@Temperature 121 °C
21

@Temperature 250 °F
Mechanical Properties Metric English Comments
Hardness, Shore A 54
54
Tensile Strength, Yield 31.4 MPa
4550 psi
Elongation at Yield 570 %
570 %
100% Modulus 0.00155 GPa
0.225 ksi
300% Modulus 0.00483 GPa
0.700 ksi
Tear Strength 34.3 kN/m
196 pli
Graves
Abrasion 50
50
NBS Index
Compression Set 21 %
21 %
Method B
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 142 °C
1.00 hour

@Temperature 287 °F
Users viewing this material also viewed the following: