Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 60 PHR Carbon Black, N-550 (FEF)

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer TSE Industries, Inc
Trade Name Millathane®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 60 PHR Carbon Black, N-550 (FEF).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and many other high performance polyurethane applications. Millathane 76 can be vulcanized by sulfur or peroxide cured systems.FormulationMillathane 76 100.0Zinc Stearate0.5Poly AC 617A1.0TP-9510.0Thanecure® ZM1.0MBTS4.0MBT2.0Sulfur1.5N-55060All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A 85
85
Tensile Strength, Yield 21.15 MPa
3067 psi
Elongation at Yield 331 %
331 %
100% Modulus 0.01097 GPa
1.591 ksi
200% Modulus 0.01789 GPa
2.595 ksi
300% Modulus 0.02056 GPa
2.982 ksi
Tear Strength 66.0 kN/m
377 pli
Taber Abrasion, mg/1000 Cycles 7.0

@Load 1.00 kg
7.0

@Load 2.20 lb
H-18 wheel
Compression Set 46.7 %

@Temperature 70.0 °C,
Time 79200 sec
46.7 %

@Temperature 158 °F,
Time 22.0 hour
Processing Properties Metric English Comments
Cure Time 10.0 min

@Temperature 154 °C
0.167 hour

@Temperature 309 °F