| Category | Polymer , Adhesive , Thermoset , Silicone , Silicone, RTV, Adhesive/Sealant Grade |
| Manufacturer | Dow Corning |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Dow Corning 730 SOLVENT RESISTANT SEALANT.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.40 g/cc @Temperature 25.0 °C |
1.40 g/cc @Temperature 77.0 °F |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 40 | 40 | |
| Tensile Strength, Ultimate | 2.07 MPa | 300 psi | |
| Elongation at Break | 200 % | 200 % | |
| Peel Strength | 2.63 kN/m | 15.0 pli |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 260 °C | 500 °F | |
| Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | |
| Brittleness Temperature | -65.0 °C | -85.0 °F |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 2.10e+13 ohm-cm | 2.10e+13 ohm-cm | |
| Dielectric Constant | 5.5 @Frequency 100 Hz |
5.5 @Frequency 100 Hz |
|
| 5.5 @Frequency 100000 Hz |
5.5 @Frequency 100000 Hz |
||
| Dielectric Strength | 13.0 kV/mm | 331 kV/in | |
| Dissipation Factor | 0.0034 @Frequency 100 Hz |
0.0034 @Frequency 100 Hz |
|
| 0.0043 @Frequency 100000 Hz |
0.0043 @Frequency 100000 Hz |
||
| Arc Resistance | 124 sec | 124 sec |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Shelf Life | 18.0 Month | 18.0 Month |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Color | White | |
| Water Resistant | yes |