Stir SpA POROCELL Z 445 ATS (PVC)

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Foam Grade
Manufacturer Stir SpA
Trade Name POROCELL
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Stir SpA POROCELL Z 445 ATS (PVC).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Application: Matt super foam for injection moldingInformation provided by STIR SpA
Physical Properties Metric English Comments
Specific Gravity 1.145 g/cc
1.145 g/cc
ISO 1183
Density 0.520 g/cc
0.0188 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 47
47
ISO 868
Tensile Strength at Break 8.74 MPa
1270 psi
ISO R 527
Elongation at Break 445 %
445 %
ISO R 527