Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Stir SpA POROCELL EZ 80 S (PVC)

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Foam Grade
Manufacturer Stir SpA
Trade Name POROCELL
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Stir SpA POROCELL EZ 80 S (PVC).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Application: Extrusion foam sealInformation provided by STIR SpA
Physical Properties Metric English Comments
Specific Gravity 1.269 g/cc
1.269 g/cc
ISO 1183
Density 0.823 g/cc
0.0297 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
ISO 868
Tensile Strength at Break 19.0 MPa
2760 psi
ISO R 527
Elongation at Break 381 %
381 %
ISO R 527
Users viewing this material also viewed the following: