Potters Industries A-Series P-0337 Soda-Lime Silica Technical Quality Solid Glass Spheres

Category Ceramic , Glass
Manufacturer Potters Industries
Trade Name A-Series
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Potters Industries A-Series P-0337 Soda-Lime Silica Technical Quality Solid Glass Spheres.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil drilling.Information provided by Potters Industries.
Physical Properties Metric English Comments
Bulk Density 1.53 g/cc
0.0554 lb/in³
Density 2.50 g/cc
0.0903 lb/in³
Particle Size 600 - 850 µm
600 - 850 µm
Particle Mesh Size 20 - 30 Mesh
20 - 30 Mesh
US Sieve
Mechanical Properties Metric English Comments
Hardness, Knoop 515

@Load 0.100 kg
515

@Load 0.221 lb
kg/mm²
Hardness, Mohs 5.0 - 6.0
5.0 - 6.0
Compressive Strength 96.5 - 248 MPa
14000 - 36000 psi
Coefficient of Friction 0.90 - 1.0
0.90 - 1.0
Optical Properties Metric English Comments
Refractive Index 1.51 - 1.52
1.51 - 1.52
Descriptive Properties Value Comments
% Round 80
Free Silica Content (%) 0
Shape spherical