Material Notes:
Description: TECHNYL ® A 217 is an unreinforced polyamide 66, heat stabilized, standard viscosity, for injection molding. It is available in black color.Benefits: This product offers all the primary properties of unreinforced polyamide 66. In addition it has improved resistance to high temperature and it can be used for components which have to withstand mid term temperature stresses. This product can also be vacuum metalized with very good surface quality and adhesion of the aluminum surface. In case of fire its smoke rate is very low. It is also complying with NFF 16-101 rating I3 F2.Available in: Asia Pacific and EuropeRegulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/EC. This grade complies with RoHS directive 2002/95/EC. Unless specified, this grade is not suitable for food contact, medical devices or toy applicationsApplications: It perfectly suits for the production of the head lamp bezels in automotive industry and connectors in electrical industry.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 40.0 MPa
5800 psi
ISO 527 Type 1A
Tensile Strength, Yield 60.0 MPa
8700 psi
ISO 527 type 1 A
Elongation at Break 200 %
200 %
ISO 527 Type 1A
Tensile Modulus 1.50 GPa
218 ksi
ISO 527 Type 1A
Flexural Strength 80.0 MPa
11600 psi
ISO 178
Flexural Modulus 1.45 GPa
210 ksi
ISO 178
Izod Impact, Notched (ISO) 10.0 kJ/m²
4.76 ft-lb/in²
ISO 180/1A
Izod Impact, Unnotched (ISO) NB
NB
ISO 180/1U
Charpy Impact Unnotched NB
NB
ISO 179/1eU
Charpy Impact, Notched 0.850 J/cm²
4.04 ft-lb/in²
ISO 179/1eA