Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

NOVA Chemicals Arcel 730 LV Resin 70% Polystyrene/30% Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , Polystyrene (PS) , Expanded Polystyrene (EPS)
Manufacturer NOVA Chemicals
Trade Name Arcel
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NOVA Chemicals Arcel 730 LV Resin 70% Polystyrene/30% Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
ARCEL advanced foam resin consists of polystyrene and polyethylene. ARCEL resin providesl toughness, flexibility and durability in a lightweight foam.The strength and flexibility of ARCEL resin creates a resilient foam that can be molded into numerous complex and intricate forms. Its lightweight construction is resistant to puncture, flaking, tearing and breaking. In addition, packaging molded with ARCEL resin provides good cushioning and easy handling, while its lightweight properties help lower freight and other packaging costs.ARCEL resin is available in low-pentane (LV) grades for customers governed by strict pentane emission laws or high-density applications.Arcel 730 LV resin can be continuously or batch expanded using conventional EPS expansion equipment. Some minor material handling modifications may be required. For molded part densities below 32 g/L (2.0 pcf), double-pass expansion will be required to attain desired bulk densities.
Physical Properties Metric English Comments
Density 0.0272 g/cc
0.000983 lb/in³
Expectation from Double Pass Expansion
0.0288 g/cc
0.00104 lb/in³
Expectation from Batch Expansion
0.0320 g/cc
0.00116 lb/in³
Expectation from Single Pass Expansion
Volatiles 8.5 %
8.5 %
Average VOC Content
Particle Size 800 - 1700 µm
800 - 1700 µm
98% within range
Descriptive Properties Value Comments
Color Natural (white)
Shape Spherical
Storage Max. 4°C (40°F)
Users viewing this material also viewed the following: