Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Amodel® ET-1001 L Polyphthalamide (PPA) Resin, at 50% RH  (discontinued **)

Category Polymer , Thermoplastic , Polyphthalamide (PPA) , Polyphthalamide (PPA), High Impact
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Solvay Specialty Polymers Amodel® ET-1001 L Polyphthalamide (PPA) Resin, at 50% RH  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
AMODEL ET-1001 L resin is an impact modified polyphthalamide (PPA) with exceptional impact strength and practical toughness. AMODEL PPA resins offer high fatigue strength, and good chemical resistance combined with good mechanical property retention over a broad temperature/ humidity range. Possible applications for AMODEL ET-1001 L resin include anti-friction and wear resistant components, and components of chemical and oil processing equipment, sporting goods, automobiles, household appliances, power tools, and safety equipment, where exceptional impact strength and high modulus are required. AMODEL ET-1001 L resin contains a lubricant for easier processing with conventional equipment and methods.Information provided by Solvay Advanced Polymers
Physical Properties Metric English Comments
Specific Gravity 1.15 g/cc
1.15 g/cc
ASTM D792
Moisture Absorption at Equilibrium 0.70 %
0.70 %
24 hours; ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength, Yield 62.0 MPa
8990 psi
ASTM D638
Elongation at Break 30 %
30 %
ASTM D638
Elongation at Yield 6.0 %
6.0 %
ASTM D638
Tensile Modulus 2.30 GPa
334 ksi
ASTM D638
Flexural Strength 110 MPa
16000 psi
ASTM D790
Flexural Modulus 2.60 GPa
377 ksi
ASTM D790
Izod Impact, Notched 9.60 J/cm
18.0 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 310 °C
590 °F
ASTM D3418