Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Amodel® AT-6115 HS Polyphthalamide (PPA), 15% Glass Fiber (Conditioned)

Category Polymer , Thermoplastic , Polyphthalamide (PPA) , Polyphthalamide (PPA), 20% Glass Fiber Reinforced
Manufacturer Solvay Specialty Polymers
Trade Name Amodel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Amodel® AT-6115 HS Polyphthalamide (PPA), 15% Glass Fiber (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Amodel® AT-6115 HS is a 15% glass-fiber reinforced, toughened grade of polyphthalamide (PPA) resin designed to possess more elongation than other 15% glass-fiber reinforced grades of Amodel resin. This grade was developed for automotive snap-fit electronic connectors. It offers high flow and short molding cycles.Features: Fast Molding Cycle; Good Mold Release; Heat Stabilized; High Elongation; High Flow; Impact Modified; LubricatedUses: Automotive Applications; Automotive Electronics; Automotive Under the Hood; Connectors; General Purpose; Housings; Industrial Applications; Industrial Parts; Machine/Mechanical Parts; Metal Replacement; Valves/Valve PartsInjection Molding Notes: Amodel® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Amodel® resins be dried prior to molding.Automotive Specifications ASTM D4000 PPA0123 G15 GB121 KD100 KN042 PN068 YI242; ASTM D6779 PA103G15; DELPHI M-4628 Color: BK324 Black; DELPHI M-4628 Color: NT Natural; FORD WSS-M4D943-A2 Color: BK324 Black; FORD WSS-M4D943-A2 Color: NT Natural; GM GMP.PPA.020 Color: BK-324 Black; GM GMP.PPA.020 Color: NT Natural; GM GMW16363P-PPA-GF15 Color: Black; GM GMW16363P-PPA-GF15 Color: Natural; ISO 1874 PA6T/66-HI, MH, 11-050, GF15Information provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
Dry; ISO 1183
Filler Content 15 %
15 %
Glass Fiber
Mechanical Properties Metric English Comments
Tensile Strength 95.8 MPa
13900 psi
ASTM D638
Elongation at Break 5.3 %
5.3 %
ASTM D638
Tensile Modulus 4.20 GPa
609 ksi
ASTM D638
Flexural Strength 115 MPa
16700 psi
ASTM D790
Flexural Modulus 3.45 GPa
500 ksi
ASTM D790
Shear Strength 44.1 MPa
6400 psi
ASTM D732
Izod Impact, Notched 0.800 J/cm
1.50 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 305 °C
581 °F
Peak; Dry; ASTM D3418
305 °C
581 °F
Dry; ISO 11357-3
Processing Properties Metric English Comments
Rear Barrel Temperature 316 - 324 °C
601 - 615 °F
Front Barrel Temperature 327 - 332 °C
621 - 630 °F
Melt Temperature 321 - 335 °C
610 - 635 °F
Mold Temperature 65.6 - 93.3 °C
150 - 200 °F
Drying Temperature 110 °C

@Time 14400 sec
230 °F

@Time 4.00 hour
Moisture Content <= 0.045 %
<= 0.045 %
Descriptive Properties Value Comments
Additive Heat Stabilizer
Impact Modifier
Lubricant
Mold Release
Availability Africa & Middle East
Asia Pacific
Europe
Latin America
North America
Color Black; Natural
Form Pellets
Processing Technique Water-Heated Mold Injection Molding
RoHS Compliance RoHS Compliant