Material Notes:
Information provided by Teknor Apex Company
Physical Properties Metric English Comments
Specific Gravity 0.910 g/cc
0.910 g/cc
+/- 0.02; ASTM D792
Melt Flow 5.4 g/10 min

@Load 2.16 kg,
Temperature 230 °C
5.4 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
ASTM D2240
Tensile Strength, Yield 9.205 MPa
1335 psi
ASTM D412
Elongation at Break 745 %
745 %
ASTM D412
Compression Set 27 %
27 %
23°C, 70 hr.; ASTM D395, Method B
62 %
62 %
70°C, 70 hr.; ASTM D395, Method B
77 %
77 %
100°C, 70 hr.; ASTM D395, Method B