Solvay RHODASURF® 860/P Surfactant

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay RHODASURF® 860/P Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Identification: ETHOXYLATED ISODECYL ALCOHOLCAS: 78330 – 20 – 8Available in: Asia Pacific, Europe, Latin America and North AmericaSolubility: Soluble in water and most polar and aromatic solvents.Applications: Detergent, emulsifier, or wetting agent in metal cleaning formulations. Iso-decyl alcohol ethoxylate. HLB = 11. Biodegradable high activity wetting agent for liquid systems and adjuvants for agrochemical formulationsInformation provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 0.990 g/cc
0.0358 lb/in³
pH 6.0 - 7.5
6.0 - 7.5
5% in water; RPG02
Thermal Properties Metric English Comments
Pour Point 3.00 °C
37.4 °F
Flash Point >= 100 °C
>= 212 °F
Processing Properties Metric English Comments
Moisture Content 0.50 %
0.50 %
RPG16
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Liquid
Composition Active
1
HLB number 12.4
Hydroxyl Number 128-138 mg KOH/g
Ionic Charge Nonionic