Solvay ALKAMIDE® C-4 Surfactant

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name ALKAMIDE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay ALKAMIDE® C-4 Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Chemical Name ETHOXYLATED COCONUT MONOETHANOLAMINECAS: 61791-08-0 Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: ALKAMIDE© C-4 is a coconut oil based alkanolamide with good detergency. ALKAMIDE© C-4 is an effective oil in water emulsifier making it well suited for household cleaners and industrial applications. ALKAMIDE© C-4 imparts viscosity and foam boosting to personal care formulations.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 0.980 g/cc
0.0354 lb/in³
Optical Properties Metric English Comments
Gardner Color Number <= 6.0
<= 6.0
RP-0138
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Clear Yellow Liquid
RP-0064
Composition Alkalinity as NaOH
<2.5%, RP-0203