Silberline Extra Fine "O" Standard Series

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Silberline
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Silberline Extra Fine "O" Standard Series.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Extra Fine "O" - is a very fine, high opacity, non-leafing aluminum pigment for solvent based industrial coatings. Due to the small particle size, this grade is well suited for imparting high opacity at low loading levels. This grade is not recommended for use with chromatic pigments, as it will not produce clean coloristic effects.Applications: General Industrial
Physical Properties Metric English Comments
Specific Gravity 1.47 g/cc
1.47 g/cc
Bulk Factor 0.081
0.081
Volatiles 35 %
35 %
Particle Size 10 µm
10 µm
Particle Mesh Size <= 325 Mesh
<= 325 Mesh
0.1% retained
Descriptive Properties Value Comments
Solvents Mineral Spirits/High Aromatic