Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Sichuan Deyang Haton® hGC51 PPS / AE Polyphenylene Sulfide

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS), Conductive
Manufacturer Sichuan Deyang Chemical Co. Ltd.
Trade Name Haton®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sichuan Deyang Haton® hGC51 PPS / AE Polyphenylene Sulfide.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Injection molding, conductiveInformation provided by Sichuan Deyang Chemical Co., LTD
Physical Properties Metric English Comments
Density 1.75 g/cc
0.0632 lb/in³
GB/T 1033.1-2008
Water Absorption 0.020 %
0.020 %
GB/T 1034-2008
Linear Mold Shrinkage, Flow 0.0010 cm/cm
0.0010 in/in
GB/T 15585-1995
Linear Mold Shrinkage, Transverse 0.0020 cm/cm
0.0020 in/in
GB/T 15585-1995
Mechanical Properties Metric English Comments
Tensile Strength 125 MPa
18100 psi
GB/T 1040.2-2006
Elongation at Break 0.30 %
0.30 %
GB/T1040.2-2006
Flexural Strength 200 MPa
29000 psi
GB/T 9341-2008
Flexural Modulus 23.5 GPa
3410 ksi
GB/T 9341-2008
Izod Impact, Notched (ISO) 7.80 kJ/m²
3.71 ft-lb/in²
GB/T 1843-2008
Thermal Properties Metric English Comments
Melting Point 280 °C
536 °F
GBT/T 19466.3-2004
Deflection Temperature at 1.8 MPa (264 psi) 268 °C
514 °F
GB/T 1634.2-2004
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Dielectric Constant 4.0
4.0
GB/T 1409-2006
Dissipation Factor 0.0010
0.0010
GB/T 1409-2006
Users viewing this material also viewed the following: