CIMBAR BariScan Elite Chemically Purified White Barium Sulfate (BaSO4)

Category Ceramic , Other Engineering Material , Additive/Filler for Polymer
Manufacturer CIMBAR Performance Minerals
Trade Name BariScan
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CIMBAR BariScan Elite Chemically Purified White Barium Sulfate (BaSO4).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
BariScan barite products are produced using a proprietary chemical process to enhance the purity of the natural barium sulfate ore. BariScan and BariScan Ultra barite meet and exceed the requirements for barium sulfate of the United States Pharmacopeia (USP) and European Pharmacopeia (EP). Barium Sulfate is Affirmed GRAS (Generally Recognized As Safe) by the US FDA (21 CFR 175.105, 175.300, 175.380, 175.390, 176.170, 177.1210, 177.1350, 177.1460, 177.2600, 182.99. BariScan barite is manufactured in Chatsworth, GA under stringent quality assurance procedures and Good manufacturing Practices (GMP). The Chatsworth Pharmaceutical Plant is registered with the US FDA as an Active Pharmaceutical Ingredients manufacturer.Information provided by Cimbar Performance Minerals.
Physical Properties Metric English Comments
Specific Gravity 4.40 g/cc
4.40 g/cc
Fineness 7.0
7.0
Hegman Fineness
Loss On Ignition <= 2.0 %
<= 2.0 %
Particle Size 1.0 µm
1.0 µm
Median
<= 12 µm
<= 12 µm
Max
Particle Mesh Size 325 Mesh
325 Mesh
100% passing
pH 5.0
5.0
Component Elements Properties Metric English Comments
Trace Metals <= 0.0010 %
<= 0.0010 %
Heavy Metals
Descriptive Properties Value Comments
BaSO4 (%) 98