Michelman® Licomer® W 485 Cationic montan emulsion

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Michelman®
Trade Name Licomer®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Michelman® Licomer® W 485 Cationic montan emulsion.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Cationic montan emulsionUsage: Licomer® W 485 is a high gloss emulsion that improves the performance of floor crystalllizers.Information provided by Michelman®
Physical Properties Metric English Comments
Specific Gravity 0.990 - 1.01 g/cc
0.990 - 1.01 g/cc
Volatiles 79 - 81 %
79 - 81 %
pH 5.0 - 6.0
5.0 - 6.0
Brookfield Viscosity <= 140 cP
<= 140 cP
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Milky white liquid
Emulsifier Charge Cationic
Solids Type Montan