Sharadaa Ceramics ZAP 013 Smart Cast Application

Category Ceramic
Manufacturer Sharadaa Ceramics
Trade Name ZAP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sharadaa Ceramics ZAP 013 Smart Cast Application.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Special Properties: Low Density, High Strength, Low Thermal ConductivityIndustry: Multi PurposeApplication: All type furnaces as a back up layer, Insulating Burner BlocksInformation provided by Sharadaa Ceramics Pvt. Ltd.
Physical Properties Metric English Comments
Bulk Density >= 1.25 g/cc
>= 0.0452 lb/in³
After Drying at 110°C
Grain Size <= 5000 µm
<= 5000 µm
Mechanical Properties Metric English Comments
Compressive Strength 6.86 MPa

@Temperature 1100 °C
996 psi

@Temperature 2010 °F
Cold Crushing
8.83 MPa

@Temperature 1300 °C
1280 psi

@Temperature 2370 °F
Cold Crushing
13.7 MPa

@Temperature 110 °C
1990 psi

@Temperature 230 °F
Cold Crushing
3.92 MPa

@Time 86400 sec
569 psi

@Time 24.0 hour
Cold Crushing
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1300 °C
2370 °F
Descriptive Properties Value Comments
Refractoriness >1500°C
Thermal Expansion 0.4
@ 1000°C, Reversible
Water Required to Mix 3-35%