Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Shakespeare Sanstat® CN125 .36mm Nylon 66 Monofilament

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66 Fiber
Manufacturer Shakespeare Company
Trade Name Sanstat®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shakespeare Sanstat® CN125 .36mm Nylon 66 Monofilament.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Sanstat CN125 nylon 6,6 monofilaments have electrically conductive carbon suffused into the surface. The filaments have a carbon coating thickness of approximately 1 micron.Information provided by Shakespeare Company.
Physical Properties Metric English Comments
Density 1.33 g/cc

@Diameter 0.360 mm
0.0480 lb/in³

@Diameter 0.0142 in
Product yield of 7370 m/kg.
Fiber Count 1360 dtex
1220 denier
Per Filament
Mechanical Properties Metric English Comments
Elongation at Break 32 %
32 %
Tenacity 0.353 N/tex
4.00 g/denier
5 kg breaking load
Thermal Properties Metric English Comments
Melting Point 254 °C
489 °F
Shrinkage 5.00 %

@Temperature 175 °C,
Time 601 sec
5.00 %

@Temperature 347 °F,
Time 0.167 hour
Electrical Properties Metric English Comments
Electrical Resistivity 9000 ohm-cm
9000 ohm-cm
Average
<= 14000 ohm-cm
<= 14000 ohm-cm
Users viewing this material also viewed the following: