| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.121 g/cc | 1.121 g/cc | ASTM D297, 15 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | >= 85 | >= 85 | ASTM D2240, Type A |
| 92 | 92 | AVG; ASTM D2240, Type A | |
| Tensile Strength at Break | >= 13.1 MPa | >= 1900 psi | ASTM D412 Method A |
| 15.29 MPa | 2218 psi | AVG; ASTM D412 Method A | |
| Tensile Strength, Yield | 8.322 MPa | 1207 psi | Stress at Elongation M25; ASTM D412 Method A |
| 11.85 MPa | 1719 psi | Stress at Elongation M50; ASTM D412 Method A | |
| 13.80 MPa | 2001 psi | Stress at Elongation M100; ASTM D412 Method A | |
| Elongation at Break | >= 80 % | >= 80 % | ASTM D412 Method A |
| 85 % | 85 % | AVG; ASTM D412 Method A | |
| Modulus of Elasticity | 0.02974 GPa | 4.314 ksi | ASTM D412 Method A |
| Shear Modulus | 0.009915 GPa | 1.438 ksi | ASTM D412 Method A |
| Secant Modulus | 0.02797 GPa | 4.056 ksi | ASTM D412 Method A |
| Tear Strength Test | 146 | 146 | (psi); ASTM D624, Die B |
| Compression Set | 13 % @Temperature 125 °C, Time 252000 sec |
13 % @Temperature 257 °F, Time 70.0 hour |
ASTM D395, Test B |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 191 °C | 375 °F | ASTM D1329 |
| Glass Transition Temp, Tg | -51.1 °C | -60.0 °F | ASTM D1329 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Strain Energy / Unit Volume at 20% Elongation (psi) | 119 |