| Category | Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) |
| Manufacturer | Seals Eastern, Inc |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Seals Eastern 7075 Ethylene-Propylene Rubber.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.05 g/cc | 1.05 g/cc | ASTM D297, 15 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | >= 62 | >= 62 | ASTM D2240, Type A |
| 73 | 73 | AVG; ASTM D2240, Type A | |
| Tensile Strength at Break | >= 10.31 MPa | >= 1496 psi | ASTM D412 Method A |
| 20.3 MPa | 2940 psi | AVG; ASTM D412 Method A | |
| Tensile Strength, Yield | >= 1.31 MPa | >= 190 psi | Stress at Elongation M50; ASTM D412 Method A |
| 1.45 MPa | 210 psi | AVG Stress at Elongation M25; ASTM D412 Method A | |
| >= 2.00 MPa | >= 290 psi | Stress at Elongation M100; ASTM D412 Method A | |
| 2.14 MPa | 310 psi | AVG Stress at Elongation M50; ASTM D412 Method A | |
| 3.93 MPa | 570 psi | AVG Stress at Elongation M100; ASTM D412 Method A | |
| Elongation at Break | >= 205 % | >= 205 % | ASTM D412 Method A |
| 410 % | 410 % | AVG; ASTM D412 Method A | |
| Modulus of Elasticity | 0.00993 GPa | 1.44 ksi | ASTM D412 Method A |
| Shear Modulus | 0.00331 GPa | 0.480 ksi | ASTM D412 Method A |
| Secant Modulus | 0.009329 GPa | 1.353 ksi | ASTM D412 Method A |
| Tear Strength Test | 134 | 134 | (psi); ASTM D624, Die B |
| Compression Set | 13 % @Temperature 100 °C, Time 79200 sec |
13 % @Temperature 212 °F, Time 22.0 hour |
ASTM D395, Test B |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Glass Transition Temp, Tg | -51.1 °C | -60.0 °F | ASTM D1329 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Strain Energy / Unit Volume at 20% Elongation (psi) | 26 |