Süd-Chemie Nanofil® SE 3010 Polymer Additive

Category Other Engineering Material , Additive/Filler for Polymer , Polymer
Manufacturer Süd-Chemie
Trade Name Nanofil®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Süd-Chemie Nanofil® SE 3010 Polymer Additive.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Application:PA 6, PA 6.6, PET, ABS, PS, PC-AlloysElectronicsElectrical PartsAutomotiveTechnical PartsImproves: Mechanical Properties, Melt Viscosity
Physical Properties Metric English Comments
Additive Loading 4.00 - 5.00 %
4.00 - 5.00 %
for 30-40% increase in Elastic Modulus in PAs
Mechanical Properties Metric English Comments
Modulus of Elasticity 2.60 - 2.80 GPa
377 - 406 ksi
30-40% better than Nylon 6 with 4-5% loading
Descriptive Properties Value Comments
Type Modified Nanoclay