Sibur ABS 0809M Molding Grade ABS Plastic

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Molded
Manufacturer Sibur
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sibur ABS 0809M Molding Grade ABS Plastic.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Shock resistant with high thermal resistance for production of structural and decorative parts and articles of technical purpose.
Physical Properties Metric English Comments
Water Absorption <= 0.30 %
<= 0.30 %
Melt Index of Compound 5.0 g/10 min
5.0 g/10 min
Mechanical Properties Metric English Comments
Elongation at Break >= 20 %
>= 20 %
Izod Impact, Notched (ISO) >= 16.0 kJ/m²
>= 7.61 ft-lb/in²
Charpy Impact, Notched 14.0 J/cm²
66.6 ft-lb/in²
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 109 °C
228 °F
Deflection temperature in bending , load unknown
Vicat Softening Point <= 110 °C
<= 230 °F
Descriptive Properties Value Comments
Impact Tension Strength >16 MPa