Category | Ceramic , Glass |
Manufacturer | Schott North America |
Trade Name | |
Port | Shanghai port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | Schott N-BAF10 Glass.pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 3.75 g/cc | 0.135 lb/in³ |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Knoop Microhardness | 620 | 620 | .1/20 |
Modulus of Elasticity | 89.0 GPa | 12900 ksi | |
Poissons Ratio | 0.271 | 0.271 | |
Shear Modulus | 35.0 GPa | 5080 ksi | calculated |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 6.20 µm/m-°C @Temperature -30.0 - 70.0 °C |
3.44 µin/in-°F @Temperature -22.0 - 158 °F |
|
7.00 µm/m-°C @Temperature 20.0 - 300 °C |
3.89 µin/in-°F @Temperature 68.0 - 572 °F |
||
Specific Heat Capacity | 0.560 J/g-°C | 0.134 BTU/lb-°F | |
Thermal Conductivity | 0.780 W/m-K | 5.41 BTU-in/hr-ft²-°F | |
Transformation Temperature, Tg | 660 °C | 1220 °F |
Optical Properties | Metric | English | Comments |
---|---|---|---|
Refractive Index | 1.67003 @Wavelength 587.6 nm |
1.67003 @Wavelength 587.6 nm |
n<sub>d</sub> |
1.67341 @Wavelength 546.1 nm |
1.67341 @Wavelength 546.1 nm |
n<sub>e</sub> | |
Transmission, Visible | 84.7 % @Thickness 10.0 mm, Wavelength 380 nm |
84.7 % @Thickness 0.394 in, Wavelength 380 nm |
|
95.9 % @Thickness 10.0 mm, Wavelength 405 nm |
95.9 % @Thickness 0.394 in, Wavelength 405 nm |
||
98.7 % @Thickness 10.0 mm, Wavelength 460 nm |
98.7 % @Thickness 0.394 in, Wavelength 460 nm |
||
99.6 % @Thickness 10.0 mm, Wavelength 580 nm |
99.6 % @Thickness 0.394 in, Wavelength 580 nm |
||
99.8 % @Thickness 10.0 mm, Wavelength 700 nm |
99.8 % @Thickness 0.394 in, Wavelength 700 nm |
||
IR Transmittance | 72.7 % @Thickness 10.0 mm, Wavelength 2500 nm |
72.7 % @Thickness 0.394 in, Wavelength 2500 nm |
|
99.2 % @Thickness 10.0 mm, Wavelength 1530 nm |
99.2 % @Thickness 0.394 in, Wavelength 1530 nm |
||
UV Transmittance | 17.6 % @Thickness 10.0 mm, Wavelength 350 nm |
17.6 % @Thickness 0.394 in, Wavelength 350 nm |
|
62.6 % @Thickness 10.0 mm, Wavelength 365 nm |
62.6 % @Thickness 0.394 in, Wavelength 365 nm |
||
72 % @Thickness 10.0 mm, Wavelength 370 nm |
72 % @Thickness 0.394 in, Wavelength 370 nm |
Chemical Properties | Metric | English | Comments |
---|---|---|---|
Acid Class, SR | 4.3 | 4.3 | |
Alkali Class, AR | 1.3 | 1.3 | |
Stain Resistance Class, FR | 0.00 | 0.00 |
Descriptive Properties | Value | Comments |
---|---|---|
B | 1 | |
Climatic Resistance Test CR | 1 | |
HG | 4 | |
K (10-6mm2/N) | 2.37 | |
Phosphate Resistance PR | 1 | |
T1013.0 (°C) | 652 | |
T107.6 (°C) | 790 |